Skip to Content

PRD2004 - 4,000A Wet Thermal Oxide/Sputter Ti-Cu 1,500A

https://shop.roguevalleymicrodevices.com/web/image/product.template/6162/image_1920?unique=f3c1ea0

Wet thermal silicon dioxide (SiO2), 0.4um (4,000A) thick, grown on silicon wafers. Substrates are cleaned in our class 100 cleanroom before processing. This is a furnace process, so oxide is grown on both surfaces of the wafer. PVD sputtered Titanium/Copper (Ti/Cu) deposited on front surface of 200mm (8 inch) diameter wafers. Ships with a film Certificate of Conformance.

Need something different? Email sales@roguevalleymicro.com for a quote.

$ 222.38 222.38 USD $ 222.38

Not Available For Sale

Limited remaining quantity available by Wafer(s).
  • -Material
  • -Diameter
  • -Type/Dopant
  • -Orientation
  • -Resistivity
  • -Thickness - W
  • -Surface Prep
  • -Flat/Notch
  • -Film Type
  • -Film Thickness
  • -Sides Processed
  • -Film Type
  • -Film Thickness
  • -Sides Processed

This combination does not exist.

-Material: Silicon
-Diameter: 200mm
-Type/Dopant: P/Boron
-Orientation: <100>
-Resistivity: >1 ohm-cm
-Thickness - W: 725+/-25um
-Surface Prep: SSP
-Flat/Notch: Notch, Semi-Standard
-Film Type: Wet Thermal Oxide, Sputter (Ti-Cu) Titanium Copper
-Film Thickness: 4,000A +/-5%, 1,500A +/-10%
-Sides Processed: Both, Front